August 9th, 2004, 20:34
#1
ADVERTISER
Silicon Bronze C642
Anyone know anything about this material?
Residual stresses and such.
-
August 9th, 2004 20:34
# ADS
Circuit advertisement
|
|
Membership in the largest desert racing community has its advantages
- Participate in Forum Discussions
- Send and Receive Private Messages
- Maintain Public Photo Albums
- Access to Groups
- User Profile in our Social Network
- Increased Access to more Sub Forums
- Reduced Online Advertisements
Join our community today |
-
August 10th, 2004, 06:31
#2
Re: Silicon Bronze C642
What is it you're trying to do with it?
No hits on Matweb for "C642"
-
August 10th, 2004, 07:15
#3
ADVERTISER
Re: Silicon Bronze C642
making some deep slots in a 3-1/2 round.
wants to move around alot after machining.
C64200 is the exact spec, gonna try to stress releive it.